Flexural Strength 524 MPa
76000 psi
Transverse Rupture
Pacific Sintered Materials F-240-S Steel Powdered Metal
Applications:Medium stressed mechanical componentsEquivalent MPIF Specification: F-0005-25All information provided by Pacific Sintered Metals.
Flexural Strength 524 MPa
76000 psi
Transverse Rupture
PSM Industries Pacific Sintered Metals Steel F-240-S Powdered Metal
Medium stressed mechanical components Equivalent MPIF Specification: F-0005-25Information Provided by Pacific Sintered Metals, a division of PSM Industries
Flexural Strength 524 MPa
76000 psi
0° stress angle
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic
CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li..