Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 55500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 383 MPa
55500 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF00C PA 66
LNP THERMOCOMP* RF00C is a compound based on Nylon 66 resin containing 60% Glass Fiber.
Flexural Strength 383 MPa
55500 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RX98372H PA 66
LNP* Thermocomp* RX98372H is a compound based on Nylon 66 resin containing Proprietary Fillers. Characteristics of this grade are: Healthcare.
Flexural Strength 383 MPa
55500 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP RX98372H PA 66
LNP* Thermocomp* RX98372H is a compound based on Nylon 66 resin containing Proprietary Fillers. Characteristics of this grade are: Healthcare.
Flexural Strength 383 MPa
55500 psi
ISO 178
BASF Ultramid® HMG14 HS BK 102 60% Glass Filled PA66 (Dry)
Description: Ultramid HMG14 HS BK-102 is a 60% glass reinforced, injection molding grade of PA66 offering high strength and stiffness. Due to inherently lower moisture absorption, Ultramid HMG14 HS ..
Copyright © lookpolymers.com All Rights Reserved