Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 56.9 MPa | 8250 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 56.9 MPa | 8250 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9130 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 56.9 MPa | 8250 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 56.9 MPa | 8250 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9130 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 56.9 MPa | 8250 psi | ASTM D790 |
Chase Plastics CP Pryme® NNA100 (Dry) ABS Polyamide Alloy Features: Good abrasion resistancePleasing surface appearanceGood chemical resistanceHigh impact resistanceHigh rigidityLow shrinkageSolvent resistanceHigh strengthGood thermal stabilityGood toughne.. |