Polymer Property : Flexural Strength = 8250 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 56.9 MPa
8250 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Flexural Strength 56.9 MPa
8250 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Starex® WR-9130 ASA, Unreinforced
Information provided by Samsung Cheil Industries.
Flexural Strength 56.9 MPa
8250 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Flexural Strength 56.9 MPa
8250 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Starex® WR-9130 ASA, Unreinforced
Information provided by Samsung Cheil Industries.
Flexural Strength 56.9 MPa
8250 psi
ASTM D790
Chase Plastics CP Pryme® NNA100 (Dry) ABS Polyamide Alloy
Features: Good abrasion resistancePleasing surface appearanceGood chemical resistanceHigh impact resistanceHigh rigidityLow shrinkageSolvent resistanceHigh strengthGood thermal stabilityGood toughne..