Mechanical Properties Metric English Comments
Flexural Strength 58.7 MPa
8510 psi
ASTM D790
Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified
General Purpose Acrylonitrile Butadiene Styrene, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples...
Flexural Strength 58.7 MPa
8510 psi
ASTM D790
PolyOne Geon™ HTX Ultra LA436G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy)
Higher gloss, wider processing window version of Geon HTX Ultra LA426G.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA436G Black 2880...