Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 59.3 MPa | 8600 psi | ASTM D790 |
PolyOne Trilliant™ HC HC3620-0040 RS Natural Polycarbonate + PBT (PC+PBT) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Flexural Strength | 59.3 MPa | 8600 psi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® NYA1000 Nylon/ABS Alloy Nylon/ABS alloy with high ductility and excellent chemical resistanceAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Strength | 59.3 MPa | 8600 psi | |
Master Bond EP126 Two Component Toughened Epoxy Adhesive System Master Bond Polymer System EP126 is a two component toughened epoxy resin based high temperature resistant adhesive system with continuous service capability at 500°F and outstanding chemical resis.. |
|||
Flexural Strength | 59.3 MPa | 8600 psi | ASTM D790 |
Americas Styrenics STYRON® 693 High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceHigh tensile strengthHigh stiffnessFood Contact CompliantUL Classification 94 HBTypical ApplicationsPackaging/Foam disposablesConsumer electronicsInformati.. |
|||
Flexural Strength | 59.3 MPa | 8600 psi | |
BCC Products BC 6004 Epoxy Surface Coat BC 6004 is a white thixotropic epoxy surface coat that has the ability to cure and bond to freshly poured wet plaster. This formulated resin compound can be applied with a brush or troweled to a thi.. |
|||
Flexural Strength | 59.3 MPa | 8600 psi | |
BCC Products BC 7136 Epoxy Casting BC7136 is a gray, low toxicity, aluminum filled, epoxy casting resin. This heat resistant system may be used at room temperature without post-curing. May be cast to a thickness of ¾ inch in non-con.. |