Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 59.3 MPa
8600 psi
ASTM D790
PolyOne Trilliant™ HC HC3620-0040 RS Natural Polycarbonate + PBT (PC+PBT)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
Flexural Strength 59.3 MPa
8600 psi
2.0 in/min; ASTM D790
LTL Color Compounds ColorFast® NYA1000 Nylon/ABS Alloy
Nylon/ABS alloy with high ductility and excellent chemical resistanceAll information provided by LTL Color Compounders, Inc.
Flexural Strength 59.3 MPa
8600 psi
Master Bond EP126 Two Component Toughened Epoxy Adhesive System
Master Bond Polymer System EP126 is a two component toughened epoxy resin based high temperature resistant adhesive system with continuous service capability at 500°F and outstanding chemical resis..
Flexural Strength 59.3 MPa
8600 psi
ASTM D790
Americas Styrenics STYRON® 693 High Heat Crystal Polystyrene
Product CharacteristicsHigh heat resistanceHigh tensile strengthHigh stiffnessFood Contact CompliantUL Classification 94 HBTypical ApplicationsPackaging/Foam disposablesConsumer electronicsInformati..
Flexural Strength 59.3 MPa
8600 psi
BCC Products BC 6004 Epoxy Surface Coat
BC 6004 is a white thixotropic epoxy surface coat that has the ability to cure and bond to freshly poured wet plaster. This formulated resin compound can be applied with a brush or troweled to a thi..
Flexural Strength 59.3 MPa
8600 psi
BCC Products BC 7136 Epoxy Casting
BC7136 is a gray, low toxicity, aluminum filled, epoxy casting resin. This heat resistant system may be used at room temperature without post-curing. May be cast to a thickness of ¾ inch in non-con..