Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 4.14 MPa | 600 psi | |
Pyrotek Pyroboard™ S1000 Roller Pyroboard™ S1000 is designed to be used throughout the preheat and cooling sections of the furnace.Information provided by Pyrotek. |
|||
Flexural Strength | 4.14 MPa | 600 psi | |
Saint-Gobain Rulon® E Grade Bearing/Seal PTFE
(discontinued **) Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of friction, and .. |
|||
Flexural Strength | 4.14 MPa | 600 psi | |
Saint-Gobain Rulon® AMR Bearing/Seal PTFE Same base material as Rulon AR but Rulon AMR contains a percentage of molybdenum disulfide for increased wear resistance and lower coefficient of friction. Typically used as a seal or gasket, Rulon .. |
|||
Flexural Strength | 4.14 MPa | 600 psi | |
Cotronics Resbond™ 901 High Temperature Ceramic Adhesive, Fiber Base Single component system with a paint consistency. |
|||
Flexural Strength | 4.14 MPa | 600 psi | |
Cotronics Resbond™ 918 High Temperature Ceramic Adhesive, One Composition |