Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 432 MPa | 62700 psi | ASTM D-790 |
PlastiComp Complet® LCF30/LGF20 – PA66 BLK Polyamide 66, 50% Long Carbon/Glass Fiber Composite PelletsInformation provided by PlastiComp, Inc. |
|||
Flexural Strength | 432 MPa | 62700 psi | ASTM D-790 |
PlastiComp Complet® LCF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |