Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastiComp Complet® LCF30/LGF20 – PA66 BLK Polyamide 66, 50% Long Carbon/Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Carbon Fiber Filled
Manufacturer PlastiComp
Trade Name Complēt®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Complet® LCF30/LGF20 – PA66 BLK Polyamide 66, 50% Long Carbon/Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Composite PelletsInformation provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D-792
Filler Content 50 %
50 %
Long Carbon/Glass Fiber
Mechanical Properties Metric English Comments
Tensile Strength 294 MPa
42600 psi
ASTM D-638
Elongation at Break 1.0 - 2.0 %
1.0 - 2.0 %
ASTM D-638
Tensile Modulus 26.9 GPa
3900 ksi
ASTM D-638
Flexural Strength 432 MPa
62700 psi
ASTM D-790
Flexural Modulus 21.38 GPa
3101 ksi
ASTM D-790
Izod Impact, Notched 3.20 J/cm
5.99 ft-lb/in
ASTM D-256
Izod Impact, Unnotched 9.61 J/cm
18.0 ft-lb/in
ASTM D-4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 254 °C
489 °F
ASTM D-648