Polymer Property : Flexural Strength = 740000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 5102 MPa
740000 psi
Hardening Temperature- 1175°C, Tempering Temperature- 565°C
Crucible Steel CPM® Rex® T15(HS), AISI T15 High Speed Steel Rex® T15(HS)
CPM Rex T15 is a super high speed steel made by the Crucible Particle Metallurgy (CPM) process. It is a tungsten type high speed containing high vanadium for excellent abrasion resistance, and cobal..