Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Crucible Steel CPM® Rex® T15(HS), AISI T15 High Speed Steel Rex® T15(HS)

Category Metal , Ferrous Metal , Carbon Steel , High Carbon Steel , Tool Steel
Manufacturer Crucible Steel
Trade Name CPM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Crucible Steel CPM® Rex® T15(HS), AISI T15 High Speed Steel Rex® T15(HS).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CPM Rex T15 is a super high speed steel made by the Crucible Particle Metallurgy (CPM) process. It is a tungsten type high speed containing high vanadium for excellent abrasion resistance, and cobalt for good red hardness. CPM Rex T15 is ideal for cutting difficult to machine materials where high frictional heating is encountered.The CPM process results in a homogeneous microstructure with a finer, more uniform carbide distribution imparting superior dimensional stability, grindability and toughness when compared to steels produced by conventional processes. The CPM process also allows the design of more highly alloyed grades which cannot be produced by conventional steelmaking.Information provided by Crucible Specialty Metals.
Physical Properties Metric English Comments
Density 8.193 g/cc
0.2960 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 245 - 275
245 - 275
Annealed
Hardness, Rockwell C 64.5
64.5
Hardening Temperature- 1175°C; Tempering Temperature- 565°C
68
68
Hardening Temperature- 1235°C; Tempering Temperature- 540°C
Modulus of Elasticity 214 GPa
31000 ksi
Flexural Strength 4005 MPa
580900 psi
Hardening Temperature- 1235°C, Tempering Temperature- 540°C
5102 MPa
740000 psi
Hardening Temperature- 1175°C, Tempering Temperature- 565°C
Charpy Impact 16.0 J
11.8 ft-lb
Hardening Temperature- 1235°C; Tempering Temperature- 540°C
29.0 J
21.4 ft-lb
Hardening Temperature- 1175°C; Tempering Temperature- 565°C
Thermal Properties Metric English Comments
CTE, linear 9.90 µm/m-°C

@Temperature 20.0 - 260 °C
5.50 µin/in-°F

@Temperature 68.0 - 500 °F
12.5 µm/m-°C

@Temperature 20.0 - 540 °C
6.94 µin/in-°F

@Temperature 68.0 - 1000 °F
Shrinkage -0.200 %

@Treatment Temp. 1205 °C
-0.200 %

@Treatment Temp. 2201 °F
Hardening
Component Elements Properties Metric English Comments
Carbon, C 1.6 %
1.6 %
Chromium, Cr 4.0 %
4.0 %
Cobalt, Co 5.0 %
5.0 %
Iron, Fe 72.28 %
72.28 %
As Remainder
Sulfur, S 0.060 - 0.22 %
0.060 - 0.22 %
Tungsten, W 12 %
12 %
Vanadium, V 4.9 %
4.9 %
Descriptive Properties Value Comments
Grindability; Metal Removed/Wheel Worn 2.2
Users viewing this material also viewed the following: