Polymer Property : Flexural Strength = 86.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 58.6 - 86.2 MPa
8500 - 12500 psi
Bulk Molding Compounds BMC T60-6009 Compression Grade Wear Resistant Molding Compound
BMC T60-6009 is a compression grade wear resistant molding compound. This material was specifically formulated for applications that require excellent abrasion resistance. Due to its low specific ..