Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 89.0 MPa | 12900 psi | ISO 178 |
SABIC Innovative Plastics LNP COLORCOMP D10006U PC LNP* COLORCOMP* D10006U is an unfilled Polycarbonate. Added features include: Lasermarking Capability, UL Listed. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ASTM D790 |
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS (Asia Pacific) LNP* Faradex* NS003 is a compound based on PC+ABS Blend resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ASTM D790M |
DSM Somos® 7120 Epoxy Photopolymer, Green Parts
(discontinued **) DescriptionDSM Somos® 7120 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u.. |
|||
Flexural Strength | >= 89.0 MPa | >= 12900 psi | |
MarkeTech Repton EXP 22 Magnesia MgO REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ASTM D790 |
LG Chemical LUCEL N109-02 General Purpose POM, Unreinforced, Externally Lubricated, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | |
Manifattura Cattaneo POM c Acetal Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RL002 PA 66 LNP LUBRICOMP* RL002 is a compound based on Nylon 66 resin containing 10% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX98477 PC LNP* STAT-KON* DX98477 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Flexural Strength | 89.0 MPa | 12900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX11355 PC (Asia Pacific) This is a PC based compound with good plating, surface, mechanical performance and flame retardant (Halogen free), a good candidate for Laser Direct Structuring applications. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp 2FL24 FP-E (EFTE) LNP* 2FL24 is a Fluoropolymer, ETFE grade containing Glass Fibers and PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ASTM D790 |
Plenco 08112 Polyester BMC, Compression Molded PLENCO 08112 is a renumber of PlasGlas 10112. PLENCO 08112 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co.. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ISO 178 |
Polyplastics Duranex® 2000 Polybutylene Terephthalate (PBT), High flow DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | Outer Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-410 A4A Polymer Alloy ZX-410 is a bearing material with excellent properties and a very affordable price.Main Characteristics: Hard, Stiff, Tough; High dimensional stability; High chemical resistance; High water resistan.. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
Zhejiang Juner PC-A2-1 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
Zhejiang Juner PC-A2-9A Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
Zhejiang Juner PC-A7-5 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ASTM D790 |
Plenco 3597 Phenolic, Granular, Injection Molded PLENCO 03597 is a mineral filled phenolic molding compound offering excellent flammability ratings even at thin cross sections, along with excellent arc and comparative track resistance values. UL r.. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | 2 mm/min; ISO 178 |
Chi Mei Kibisan® PN-117C SAN High Clarity |
|||
Flexural Strength | 89.0 MPa | 12900 psi | 2 mm/min; ISO 178 |
Chi Mei Polyrex® PG-383 Polystyrene High heat; high strength |
|||
Flexural Strength | 89.0 MPa | 12900 psi | ISO 178 |
Eurostar Star L PA66 D61 PA66, Injection Molded Star L PA66 D51 is a PTFE/Silicone Oil Lubricated, Unreinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 89.0 MPa @Temperature 120 °C |
12900 psi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry) Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st.. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
Zhejiang Juner PC-A1-1 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
Zhejiang Juner PC-A1-11 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
Zhejiang Juner PC-A1-18 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
Zhejiang Juner PC-A1-2 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
Zhejiang Juner PC-A1-3 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
Zhejiang Juner PC-A1-33 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
Zhejiang Juner PC-A1-9 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 89.0 MPa | 12900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON KX97157 Acetal Copolymer (Europe-Africa-Middle East) LNP* STATKON* KX97157 is a compound based on Acetal resin containing Carbon. Added features include : Electrically Conductive, Impact Modified. |