Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 3597 Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 3597 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 03597 is a mineral filled phenolic molding compound offering excellent flammability ratings even at thin cross sections, along with excellent arc and comparative track resistance values. UL recognized under component file E40654. 03597 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.640 g/cc
0.0231 lb/in³
ASTM D1895
Density 1.55 g/cc
0.0560 lb/in³
ASTM D792
Water Absorption 0.111 %
0.111 %
ASTM D570
Linear Mold Shrinkage 0.0075 cm/cm
0.0075 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 79
79
ASTM D785
Tensile Strength, Ultimate 52.0 MPa
7540 psi
ASTM D638
Elongation at Break 0.50 %
0.50 %
ASTM D638
Tensile Modulus 11.3 GPa
1640 ksi
ASTM D638
Flexural Strength 89.0 MPa
12900 psi
ASTM D790
Flexural Modulus 9.80 GPa
1420 ksi
ASTM D790
Compressive Strength 180 MPa
26100 psi
ASTM D695
Izod Impact, Notched 0.164 J/cm
0.307 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.173 J/cm²
0.823 ft-lb/in²
ASTM D256
Impact 93
93
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 48.0 µm/m-°C

@Temperature 40.0 - 130 °C
26.7 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.530 W/m-K

@Temperature 100 °C
3.68 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 206 °C
403 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 162 °C
324 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 0.510 mm
V-0

@Thickness 0.0201 in
Oxygen Index 39 %
39 %
ASTM D2863
Shrinkage 0.14 %
0.14 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.20e+12 ohm-cm
2.20e+12 ohm-cm
ASTM D247
Dielectric Constant 4.7
4.7
ASTM D150
Dielectric Strength 10.0 kV/mm
254 kV/in
Step by Step; ASTM D149
13.4 kV/mm
340 kV/in
Short Time; ASTM D149
Dissipation Factor 0.046
0.046
ASTM D150
Arc Resistance 185 sec
185 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638