Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 89.66 MPa | 13000 psi | ASTM D790 |
Lucent Polymers PC/PBT-1231 Polycarbonate+PBT, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 89.66 MPa | 13000 psi | ASTM D790 |
Lucent Polymers POM-100 Acetal Copolymer, General Purpose, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 89.66 MPa | 13000 psi | ASTM D790 |
Lucent Polymers POM-270 Acetal Copolymer, Easy Flow, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |