Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucent Polymers POM-100 Acetal Copolymer, General Purpose, Injection Grade

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Lucent Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucent Polymers POM-100 Acetal Copolymer, General Purpose, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.022 cm/cm

@Thickness 3.17 mm
0.022 in/in

@Thickness 0.125 in
1/8" Section
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.69 MPa
8802 psi
ASTM D638
Elongation at Break >= 30 %
>= 30 %
ASTM D638
Flexural Strength 89.66 MPa
13000 psi
ASTM D790
Flexural Modulus 2.414 GPa
350.1 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
1.30 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 160 - 165 °C
320 - 329 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 132.22 °C
270.00 °F
ASTM D648
Users viewing this material also viewed the following: