Polymer Property : Flexural Strength = 9.03 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 9.03 MPa
1310 psi
ASTM D790
Aclo Accucomp Polyethylene LD0102L Low Density
Flexural Strength 9.03 MPa
1310 psi
ASTM D790
Aclo Accucomp Polyethylene LD0109L Low Density