Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 62.7 MPa | 9090 psi | 1.3 mm/min; ASTM D790 |
PolyOne LubriOne™ AT-000/18T 2S Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Strength | 62.7 MPa | 9090 psi | ASTM D790 |
PolyOne Geon™ SF M7000 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 62.7 MPa | 9090 psi | ASTM D790 |
PolyOne Geon™ SF M7010 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 62.7 MPa | 9090 psi | ASTM D790 |
PolyOne Geon™ SF M7020 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |