Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 65.5 MPa | 9500 psi | |
Protective Coating PC-Rot Terminator® Epoxy Wood Consolidant Description: PC-Rot Terminator® is designed to strengthen decayed or rotted wood. The mixture is a low viscosity liquid that penetrates porous surfaces filling and sealing voids with an epoxy that .. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Polymer Resources ABS-G5 ABS, 5% Glass Reinforced Acrylonitrile Butadiene Styrene, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Polymer Resources ABS-G5-[color]-3 ABS, 5% Glass Reinforced, UV-stabilized Acrylonitrile Butadiene Styrene, 5% Glass Reinforced, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Polymer Resources TP-FR IM2 PBT, Impact Modified, Flame Retardant, High Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Polymer Resources TP-FR-IM2-[color]-6 Polybutylene Terephthalate, Low Temperature Impact Modified, Flame Retardant Polybutylene Terephthalate, Low Temperature Impact Modified, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Flexural Strength | 65.5 MPa @Thickness 3.17 mm |
9500 psi @Thickness 0.125 in |
ASTM D790 |
PTS Trilac® FR3800 Flame Retardant ABS Resin, RoHS Compliant Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
PolyOne Stat-Tech™ AS-10SS/000 ABS - 10% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790-1 |
Premix Premi-Glas® 8105 Glass Reinforced Polyester BMC
(discontinued **) Description: Premi-Glas® 8105 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Fiberfil® J-61/20/E Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM HS L BK Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUL File Number: E157318Processing Method: In.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM L Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM L N Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES Plastiblend® PA6/ABS 1120 B1 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES Plastiblend® PBT/ABS BK Availability: North AmericaForms: PelletsAppearance: BlackTPCI# 6722121Information provided by TP Composites, Inc. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | Type I, 1.3 mm/min; ASTM D790 |
Styron MAGNUMâ„¢ 347 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D 790 |
Saint-Gobain Meldin® 1380 Thermoplastic Bearing Material Specify Meldin 1380 for use with soft mating surfaces that gall easily, such as stainless steel or aluminum. Meldin 1380 also complies with the FDA Title 21 CFR regulations for contact with article.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D-790 |
Axiall UV-6680 Rigid PVC, Molding Georgia Gulf UV-6680 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, such as .. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Americas Styrenics EA3130 High Heat Crystal Polystyrene Product CharacteristicsAdditive FreeFood Contact CompliantTypical ApplicationsMedical PartsColor Concentrate CarrierLow Profile AdditivesInformation provided by AmericasStyrenics LLC. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Adell ZS-30 Nylon/Olefin Alloy Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790-95 |
Multibase Multi-ABS 3246 High Flow Grade Data provided by Multibase. |