Polymer Property : Clash Berg Modulus = 0.310 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Clash Berg Modulus 0.310 GPa

@Temperature -22.0 °C
45.0 ksi

@Temperature -7.60 °F
ASTM D1043
PolyOne Geon™ Vinyl Flexible B4D01 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Clash Berg Modulus 0.310 GPa

@Temperature -51.0 °C
45.0 ksi

@Temperature -59.8 °F
ASTM D1043
PolyOne Geon™ Vinyl Flexible B65B1 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Clash Berg Modulus 0.310 GPa

@Temperature -55.0 °C
45.0 ksi

@Temperature -67.0 °F
ASTM D1043
PolyOne Geon™ Vinyl Flexible 82024 Polyvinyl Chloride, Flexible (PVC, Flexible)
Automotive OEM approval(s).Information provided by PolyOne