Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 175 kN/m | 999 pli | Die C; ASTM D642-54 |
DuPont Performance Polymers Hypalon® 45 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound
(d Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato.. |
|||
Graves Tear Strength | 175 kN/m | 1000 pli | Die C; ASTM D624 |
Lubrizol ESTANE® 58244 Ether Based Thermoplastic Polyurethane Features: Non-Halogenated flame retardant compoundUses: Extrusion – wire and cable and general extrusion where flame retardant propertied are requiredAvailable in Americas, Europe, Middle East, Afr.. |
|||
Graves Tear Strength | 175 kN/m | 1000 pli | Die C; ASTM D624 |
Lubrizol ESTANE® ETE60DS3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, high transparencyUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket; Injection molding: VariousAvailable in.. |