Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 33.3 kN/m | 190 pli | PVC (70)/CP80AS2(30) |
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H.. |
|||
Graves Tear Strength | 33.3 kN/m @Temperature 23.9 °C |
190 pli @Temperature 75.0 °F |
Die C; ASTM D624 |
Advanced Polymer Alloys Alcryn® 2080 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Graves Tear Strength | 33.3 kN/m @Temperature 23.9 °C |
190 pli @Temperature 75.0 °F |
Die C; ASTM D624 |
Advanced Polymer Alloys Alcryn® 4660 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |