Mechanical Properties Metric English Comments
Graves Tear Strength 47.3 kN/m
270 pli
PVC (50)/CP80AS2(50)
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane
Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H..
Graves Tear Strength 47.3 kN/m
270 pli
Die C; ASTM D624
Lubrizol Estane® 58252 Thermoplastic Polyurethane
Type: Estane® 58252 is a 70A polyether-type thermoplastic polyurethane (TPU).Features: Formulated to have one of the highest MVT values within the thermoplastic polyurethane class. It is also amon..
Graves Tear Strength 47.3 - 245 kN/m
270 - 1400 pli
Average value: 104 kN/m Grade Count:9
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a..