Mechanical Properties Metric English Comments
Graves Tear Strength 28.6 kN/m

@Temperature 24.0 °C
163 pli

@Temperature 75.2 °F
Die C; ASTM D624
Advanced Polymer Alloys DuraGrip™ 6070 BK Thermoplastic Elastomer
DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in the injection molding process. DGR 6070NC has an excellent soft touch feel, will bond t..