Polymer Property : Graves Tear Strength = 55.2 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Graves Tear Strength 55.2 kN/m
315 pli
Die C; ASTM D624
Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane
Features: Very high tensile strength, excellent low temperature flexibility, and superior abrasion and cut resistanceUses: Extrusion – Wire and cable, Hose and tube & General purposeAvailable in Am..