Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 102 kN/m | 583 pli | Die C; ASTM D624 |
Lubrizol Estane® ZHF 90AT0 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 90AT0 TPU is a clear, glossy, zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding TPU properties.Uses: Cable jacket and tube/hos.. |