Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 60.0 - 150 kN/m | 342 - 856 pli | Average value: 92.5 kN/m Grade Count:6 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |