Mechanical Properties Metric English Comments
Compressive Yield Strength 0.0138 - 0.0689 MPa

@Strain 25.0 %
2.00 - 10.0 psi

@Strain 25.0 %
0.2"/min. strain rate
Rogers Corporation Poron® Shock Seal™ 4790-79-15 Urethane Foam, Industrial Grade
Thickness: 0.125"- 0.500"Color: BlackInformation provided by Rogers Corporation.
Compressive Yield Strength 0.0138 MPa

@Strain 25.0 %
2.00 psi

@Strain 25.0 %
0.2"/min. strain rate
Rogers Corporation Poron® Shock Seal™ 4790-79-9 Handheld Urethane Foam, Handheld Grade, PET Reinforced
Extreme Impact Protection, Ultimate ReliabilitySpecifically engineered to protect sensitive components from damage caused by impactConsistent cushioning performance through repeated impactsExcellent..
Compressive Yield Strength 0.0138 MPa
2.00 psi
at 1% Comp., RT, Parallel to Thickness
Zircar Ceramics Z-MAG/2300 Soluble Fiber Insulation
ZIRCAR NON-RCF Insulation Type Z-MAG/2300 is a rigid combination of soluble NON-RCF silica magnesia glass fibers and inorganic binder. It is suitable for use as a substitute for insulation containin..