Polymer Property : Compressive Yield Strength = 0.207 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.207 - 0.415 MPa
30.0 - 60.2 psi
at 25% deflection; 0.2"/min strain rate
Rogers Corporation Poron® 4701-50-30 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4..
Compressive Yield Strength 0.207 MPa
30.0 psi
2% compression
Zircar Zirconia Buster M-15 Alumina Boards, Discs & Cylinders Insulation
Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite..
Compressive Yield Strength 0.207 MPa
30.0 psi
2% compression
Zircar Zirconia Buster M-15 Alumina Boards, Discs & Cylinders Insulation
Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite..