Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.207 - 0.415 MPa | 30.0 - 60.2 psi | at 25% deflection; 0.2"/min strain rate |
Rogers Corporation Poron® 4701-50-30 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4.. |
|||
Compressive Yield Strength | 0.207 MPa | 30.0 psi | 2% compression |
Zircar Zirconia Buster M-15 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Compressive Yield Strength | 0.207 MPa | 30.0 psi | 2% compression |
Zircar Zirconia Buster M-15 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |