Mechanical Properties Metric English Comments
Compressive Yield Strength 0.720 MPa
104 psi
at 20% deflection; ASTM D3574C
Mearthane Durethaneâ„¢ F DF-640A Closed Cell Foam Polyurethane
MDI backbone: ester.Shore 00 Hardness: 85Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient..
Compressive Yield Strength 0.720 MPa
104 psi
at 20% deflection; ASTM D3574C
Mearthane Durethaneâ„¢ M DM-650A Foam Polyurethane
MDI backbone: ester.Shore 00 Hardness: 95Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur..