Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 771 MPa @Temperature 23.0 °C |
112000 psi @Temperature 73.4 °F |
prEN2580 Type A |
Hexcel® HexPly® M35-4 80-180°C Curing Epoxy Matrix, M35-4/40%/G803/1200 Fabric Fiber: T300 3K, 285 g/m2Information provided by HexCel |