Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 912 MPa | 132000 psi | Results normalized to 60% fibre volume for Carbon, 50% fibre volume for Kevlar; EFA TP-003 |
Hexcel® HexPly® 920CX-940-42% 125°C Curing Epoxy Matrix Intermediate modulus, 6K carbon, 5H satin, 285 g/m2Information provided by HexCel |