Compressive Yield Strength 912 MPa
132000 psi
Results normalized to 60% fibre volume for Carbon, 50% fibre volume for Kevlar; EFA TP-003
Hexcel® HexPly® 920CX-940-42% 125°C Curing Epoxy Matrix
Intermediate modulus, 6K carbon, 5H satin, 285 g/m2Information provided by HexCel