Mechanical Properties Metric English Comments
Compressive Yield Strength 9.928 MPa
1440 psi
Abatron AboCast 50-16/AboCure 50-17 Epoxy
Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/28 ratio. Pot life: 500 g, 29 min. at 70°C (160°F). Exothermic Peak 242°C (468°F). Cures in 1-2 hrs at ..