Abatron AboCast 50-16/AboCure 50-17 Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Abatron
Trade Name AboCast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 50-16/AboCure 50-17 Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/28 ratio. Pot life: 500 g, 29 min. at 70°C (160°F). Exothermic Peak 242°C (468°F). Cures in 1-2 hrs at 80-100°C (175-212°F) + 1-3 hrs at 120-160°C (250-320°F). For large castings: 8-24 hrs at RT until hard + 1-2 hrs at 80°C (175°F) + 1-2 hrs at 100°C (212°F) + 1-2 hrs at 120°C (250°F) + (optional) 1-2 hrs at 150-160°C (300-355°F). Do not demold before 100°C cure cycle.
Physical Properties Metric English Comments
Viscosity Measurement 60

@Temperature 70.0 °C
60

@Temperature 158 °F
Mechanical Properties Metric English Comments
Hardness, Rockwell M 96
96
Tensile Strength, Ultimate 79.22 MPa
11490 psi
Elongation at Break 18.2 %
18.2 %
Flexural Yield Strength 131 MPa
19000 psi
Flexural Modulus 3.45 GPa
500 ksi
Compressive Yield Strength 9.928 MPa
1440 psi
Compressive Modulus 1.86 GPa
270 ksi
Izod Impact, Notched 0.363 J/cm
0.680 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 102 °C
216 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.22e+16 ohm-cm
>= 1.22e+16 ohm-cm
Surface Resistance >= 7.85e+15 ohm
>= 7.85e+15 ohm
Dielectric Constant 3.41

@Frequency 1e+6 Hz
3.41

@Frequency 1e+6 Hz
3.75

@Frequency 1000 Hz
3.75

@Frequency 1000 Hz
3.78

@Frequency 60 Hz
3.78

@Frequency 60 Hz
Dissipation Factor 0.0052

@Frequency 60 Hz
0.0052

@Frequency 60 Hz
0.0092

@Frequency 1000 Hz
0.0092

@Frequency 1000 Hz
0.031

@Frequency 1e+6 Hz
0.031

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Pot Life 29.0 min

@Temperature 70.0 °C
29.0 min

@Temperature 158 °F
500 g
Descriptive Properties Value Comments
Exotherm 242°C
Peak