Polymer Property : Compressive Yield Strength = 17000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 36.5 - 117 MPa
5300 - 17000 psi
Average value: 102 MPa Grade Count:8
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
Compressive Yield Strength 100 - 117 MPa
14500 - 17000 psi
Average value: 111 MPa Grade Count:3
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..