Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.07 - 1.67 g/cc
0.0385 - 0.0603 lb/in³
Average value: 1.24 g/cc Grade Count:133
Filler Content 5.00 - 15.0 %
5.00 - 15.0 %
Average value: 11.2 % Grade Count:33
Water Absorption 0.0900 - 8.30 %
0.0900 - 8.30 %
Average value: 2.50 % Grade Count:59
2.60 - 3.40 %

@Temperature 70.0 - 70.0 °C
2.60 - 3.40 %

@Temperature 158 - 158 °F
Average value: 3.00 % Grade Count:2
Moisture Absorption at Equilibrium 1.20 - 3.00 %
1.20 - 3.00 %
Average value: 2.13 % Grade Count:22
Water Absorption at Saturation 7.00 - 9.50 %
7.00 - 9.50 %
Average value: 8.30 % Grade Count:11
Viscosity 2.60 - 50.0 cP
2.60 - 50.0 cP
Average value: 18.4 cP Grade Count:3
Linear Mold Shrinkage 0.00100 - 0.0200 cm/cm
0.00100 - 0.0200 in/in
Average value: 0.00629 cm/cm Grade Count:115
0.00500 - 0.00500 cm/cm

@Temperature 80.0 - 80.0 °C
0.00500 - 0.00500 in/in

@Temperature 176 - 176 °F
Average value: 0.00500 cm/cm Grade Count:1
Linear Mold Shrinkage, Transverse 0.00680 - 0.100 cm/cm
0.00680 - 0.100 in/in
Average value: 0.0157 cm/cm Grade Count:24
0.00900 - 0.00900 cm/cm

@Temperature 80.0 - 80.0 °C
0.00900 - 0.00900 in/in

@Temperature 176 - 176 °F
Average value: 0.00900 cm/cm Grade Count:1
Melt Flow 2.00 - 93.8 g/10 min
2.00 - 93.8 g/10 min
Average value: 17.8 g/10 min Grade Count:15
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100 - 122
100 - 122
Average value: 119 Grade Count:37
Hardness, Shore D 73.0 - 81.0
73.0 - 81.0
Average value: 77.3 Grade Count:4
Ball Indentation Hardness 95.0 - 155 MPa
13800 - 22500 psi
Average value: 127 MPa Grade Count:3
Tensile Strength, Ultimate 3.45 - 165 MPa
500 - 23900 psi
Average value: 95.5 MPa Grade Count:92
20.0 - 170 MPa

@Temperature -40.0 - 121 °C
2900 - 24700 psi

@Temperature -40.0 - 250 °F
Average value: 70.7 MPa Grade Count:7
27.5 - 52.5 MPa

@Temperature 130 - 175 °C
3990 - 7610 psi

@Temperature 266 - 347 °F
Average value: 70.7 MPa Grade Count:2
27.5 - 52.5 MPa

@Time 1.80e+7 - 7.20e+7 sec
3990 - 7610 psi

@Time 5000 - 20000 hour
Average value: 70.7 MPa Grade Count:2
Tensile Strength, Yield 51.7 - 170 MPa
7500 - 24700 psi
Average value: 103 MPa Grade Count:50
Elongation at Break 2.00 - 30.0 %
2.00 - 30.0 %
Average value: 5.53 % Grade Count:107
2.00 - 30.0 %

@Temperature -40.0 - 121 °C
2.00 - 30.0 %

@Temperature -40.0 - 250 °F
Average value: 9.69 % Grade Count:7
Elongation at Yield 1.60 - 15.0 %
1.60 - 15.0 %
Average value: 4.93 % Grade Count:21
Modulus of Elasticity 1.90 - 16.0 GPa
276 - 2320 ksi
Average value: 4.99 GPa Grade Count:57
1.445 - 6.90 GPa

@Temperature -40.0 - 120 °C
209.6 - 1000 ksi

@Temperature -40.0 - 248 °F
Average value: 3.52 GPa Grade Count:6
Flexural Yield Strength 13.8 - 250 MPa
2000 - 36300 psi
Average value: 142 MPa Grade Count:122
49.987 - 265 MPa

@Temperature -40.0 - 121 °C
7250.0 - 38400 psi

@Temperature -40.0 - 250 °F
Average value: 147 MPa Grade Count:5
Flexural Modulus 1.52 - 24.0 GPa
220 - 3480 ksi
Average value: 4.53 GPa Grade Count:124
0.992845 - 5.19865 GPa

@Temperature -40.0 - 121 °C
144.002 - 754.012 ksi

@Temperature -40.0 - 250 °F
Average value: 2.30 GPa Grade Count:3
Compressive Yield Strength 100 - 117 MPa
14500 - 17000 psi
Average value: 111 MPa Grade Count:3
Izod Impact, Notched 0.427 - 1.95 J/cm
0.800 - 3.65 ft-lb/in
Average value: 0.720 J/cm Grade Count:79
0.37373 - 0.400 J/cm

@Temperature -40.0 - -40.0 °C
0.70015 - 0.749 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.391 J/cm Grade Count:3
Izod Impact, Unnotched 0.481 - 5.34 J/cm
0.900 - 10.0 ft-lb/in
Average value: 4.30 J/cm Grade Count:14
Izod Impact, Notched (ISO) 3.80 - 12.0 kJ/m²
1.81 - 5.71 ft-lb/in²
Average value: 6.65 kJ/m² Grade Count:18
5.00 - 8.00 kJ/m²

@Temperature -30.0 - -30.0 °C
2.38 - 3.81 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 6.50 kJ/m² Grade Count:2
Izod Impact, Unnotched (ISO) 20.0 - 70.0 kJ/m²
9.52 - 33.3 ft-lb/in²
Average value: 44.8 kJ/m² Grade Count:8
38.0 - 38.0 kJ/m²

@Temperature -30.0 - -30.0 °C
18.1 - 18.1 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 38.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 2.00 J/cm² - NB
9.52 ft-lb/in² - NB
Average value: 5.12 J/cm² Grade Count:32
1.50 J/cm² - NB

@Temperature -40.0 - -20.0 °C
7.14 ft-lb/in² - NB

@Temperature -40.0 - -4.00 °F
Average value: 3.83 J/cm² Grade Count:19
Charpy Impact, Notched 0.100 - 2.20 J/cm²
0.476 - 10.5 ft-lb/in²
Average value: 0.924 J/cm² Grade Count:39
0.100 - 20.0 J/cm²

@Temperature -40.0 - -20.0 °C
0.476 - 95.2 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 2.00 J/cm² Grade Count:24
Thermal Properties Metric English Comments
CTE, linear 28.0 - 97.0 µm/m-°C
15.6 - 53.9 µin/in-°F
Average value: 46.2 µm/m-°C Grade Count:35
CTE, linear, Transverse to Flow 12.0 - 93.0 µm/m-°C
6.67 - 51.7 µin/in-°F
Average value: 72.3 µm/m-°C Grade Count:7
Electrical Properties Metric English Comments
Electrical Resistivity 1.00 - 1.00e+17 ohm-cm
1.00 - 1.00e+17 ohm-cm
Average value: 2.63e+15 ohm-cm Grade Count:46
Surface Resistance 10.0 - 3.10e+15 ohm
10.0 - 3.10e+15 ohm
Average value: 3.01e+14 ohm Grade Count:17
Insulation Resistance 10000 - 1.00e+11 ohm
10000 - 1.00e+11 ohm
Average value: 3.33e+10 ohm Grade Count:3
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:4
Shielding Effectiveness 50.0 dB
50.0 dB
Average value: 50.0 dB Grade Count:3
Dielectric Constant 2.60 - 7.00
2.60 - 7.00
Average value: 3.90 Grade Count:12
Dielectric Strength 11.0 - 80.0 kV/mm
280 - 2030 kV/in
Average value: 23.9 kV/mm Grade Count:27
Dissipation Factor 0.0100 - 0.0700
0.0100 - 0.0700
Average value: 0.0292 Grade Count:11
Arc Resistance 112 - 160 sec
112 - 160 sec
Average value: 131 sec Grade Count:5
Comparative Tracking Index 225 - 600 V
225 - 600 V
Average value: 488 V Grade Count:16
Users viewing this material also viewed the following: