Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 175 MPa | 25400 psi | ISO 604 |
Hexcel® HexPly® 924 180°C Curing Epoxy Matrix HexPly® 924 is a controlled flow epoxy matrix developed for the fabrication of high temperature resistant primary structures. When cured, HexPly® 924 becomes a tough composite with high impact res.. |
|||
Compressive Yield Strength | 175 MPa | 25400 psi | ISO 604 |
Hexcel® HexPly® M20 266°F (130°C) Curing Epoxy Matrix M20 was designed to meet need for high temperature performance combined with a low energy cure cycle. Suitable for aircraft primary and secondary structures, and composite repair.Information provi.. |
|||
Compressive Yield Strength | 175 MPa | 25400 psi | 10% Strain; EN ISO 604 |
Ensinger TECASINT 1021 Polyimide, 15% Graphite Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |