Mechanical Properties Metric English Comments
Compressive Yield Strength 148 - 241 MPa
21500 - 35000 psi
Average value: 193 MPa Grade Count:5
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..