Mechanical Properties Metric English Comments
Compressive Yield Strength 151 MPa
21900 psi
ASTM D695
Westlake Plastics Tempalux® Polyetherimide
An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad ..
Compressive Yield Strength 151 MPa
21900 psi
ASTM D695
Westlake Plastics Tempalux® Polyetherimide For Medical Applications
Medical grade Tempalux is made from Ultem® polyetherimide resin, an amorphous thermoplastic which exhibits excellent resistance to a wide range of chemicals and disinfectants. Ultem maintains its ..