Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake Plastics Tempalux® Polyetherimide

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer Westlake Plastics
Trade Name Tempalux®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Tempalux® Polyetherimide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad chemical resistance. Tempalux stock shapes are inherently flame resistant with low smoke emission. Tempalux stock shapes display property retention and resistance to environmental stress cracking when exposed to a wide variety of chemicals. The standard color of Tempalux stock shapes is light amber. Glass filled grades appear tan or greenish in color. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Water Absorption 0.25 %
0.25 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Hardness, Rockwell M 109
109
ASTM D7852
Tensile Strength, Yield 105 MPa
15200 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Tensile Modulus 2.96 GPa
430 ksi
ASTM D638
Flexural Yield Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 3.31 GPa
480 ksi
ASTM D790
Compressive Yield Strength 151 MPa
21900 psi
ASTM D695
Compressive Modulus 3.31 GPa
480 ksi
ASTM D695
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 13.3 J/cm
25.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 55.8 µm/m-°C

@Temperature 20.0 °C
31.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.220 W/m-K
1.53 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ASTM D648
Flammability, UL94 5VA

@Thickness 1.91 mm
5VA

@Thickness 0.0750 in
Oxygen Index 47 %
47 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Dielectric Constant 3.15

@Frequency 1000 Hz
3.15

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 32.7 kV/mm
831 kV/in
ASTM D149
Dissipation Factor 0.0013

@Frequency 1000 Hz
0.0013

@Frequency 1000 Hz
ASTM D150