Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 22.0 MPa | 3190 psi | at 5% nominal strain; ISO 604 |
Quadrant EPP Cestilene™ HD 500 R Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |