Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 22.0 MPa
3190 psi
at 5% nominal strain; ISO 604
Quadrant EPP Cestilene™ HD 500 R Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.