Polymer Property : Compressive Yield Strength = 225 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 195 - 225 MPa
28300 - 32600 psi
Average value: 211 MPa Grade Count:4
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor..