Polymer Property : Compressive Yield Strength = 23890 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 164.7 MPa
23890 psi
ASTM D695
Plenco 50130 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 50130 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in natural and black.Informat..