Polymer Property : Compressive Yield Strength = 31000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 214 MPa
31000 psi
ASTM D695
Sumitomo Bakelite North America 1907-1 / 1907B-1 Glass Reinforced Hardware Grade Epoxy
Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc.
Compressive Yield Strength 214 MPa
31000 psi
90º, RT, Dry; DIN65380
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Information provided by HexCel