Compressive Yield Strength 140 - 222 MPa
20300 - 32200 psi
Average value: 166 MPa Grade Count:11
Overview of materials for Nylon 6, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E..