Polymer Property : Compressive Yield Strength = 32970 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 227.3 MPa
32970 psi
ASTM D695
Plenco Valite 697-A Novolac Phenolic, Granular, Compression Molded  (discontinued **)
This Valite product has been replaced by Plenco 7697. Data provided by Plenco.VALITE 697-A is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for ..